Akemi AKEPOX® 1005 — Highly Fluid 2-Component Epoxy for Strengthening & Filling Natural Stone

Precio normal $158.60 USD
Los gastos de envío se calcularán al momento de pagar.


Ships same day from Sterling, VA on orders placed before 12 PM ET. Questions about fit or use? Call 703-957-4544.

Buying for a business? Trade pricing is on dynamicstonetools.net.

Descripción

Akemi AKEPOX® 1005 — Highly Fluid 2-Component Epoxy for Strengthening & Filling Natural Stone

AKEPOX® 1005 is a very fluid, solvent-free, 2-component epoxy resin system with a modified amine hardener, used to firmly close cracks and pores in natural stone. Its low viscosity gives it highly penetrative properties, and the clear, light-transparent cure makes it best suited to light natural stone. The hardened resin is weather-resistant, has excellent grinding and polishing properties, increases the firmness and surface quality of the stone, and — when properly applied — is classified as harmless to health for bonded natural and artificial stone in contact with food.

Property Detail
Brand Akemi
Manufacturer AKEMI GmbH, Nürnberg, Germany
Article Number 10676 (EPOX.10676)
Product Type 2-component epoxy resin system (modified amine hardener)
Colour Light transparent
Consistency Very fluid / highly liquid (low viscosity, penetrative)
Mixing Ratio 4:1 by weight (e.g. 100 g A : 25 g B) — or 7:2 by volume (175 ml : 50 ml)
Density Comp. A 1.13 g/cm³; Comp. B 1.00 g/cm³
Consumption approx. 100–200 g/m²
Working Time (125 g) 15°C (59°F): 30–35 min; 20°C (68°F): 20–25 min; 30°C (86°F): 5–10 min; 40°C (104°F): 3–5 min
Working Time (at 20°C by amount) 25 g: 25–30 min; 125 g: 20–25 min; 1250 g: 15–20 min
Grind/Polish Ready approx. 24 h at 20°C (68°F) room temperature; approx. 3 h at 60°C (140°F) if stone pre-warmed
Hardening (pre-warmed stone) 30°C: 12 h; 40°C: 6 h; 50°C: 4 h; 60°C: 3 h
Minimum Processing Temperature Not below 15°C (59°F)
Colouring AKEPOX® Colouring Concentrates or Stone Ink, max. 5%
Bending Strength 60–70 N/mm² (approx. 8,700–10,150 psi)
Tensile Strength 35–40 N/mm² (approx. 5,075–5,800 psi)
Food Contact Classified harmless to health for bonded natural/artificial stone in contact with food when properly applied
UV / Weathering Weather-resistant; minimal tendency to yellow under UV or warmth
Solvent Content Solvent-free
Shelf Life At least 24 months stored dry and cool (5–25°C / 41–77°F) in the closed original container
Packaging 1250 g (2-component, 2 cans)
Usage For professional use only
  • Very low viscosity — highly penetrative for closing cracks and pores
  • Hardens relatively quickly and cures clear, light-transparent
  • Excellent grinding and polishing properties
  • Increases the firmness and improves the surface quality of natural stone
  • Solvent-free and weather-resistant with minimal tendency to yellow
  • Food-safe cured bond when correctly applied (externally tested)
  • Colour with AKEPOX® Colouring Concentrates or Stone Ink up to 5%

Mainly used in the stone-processing industry to strengthen porous and fissured natural stone slabs, concrete and concrete ashlar and to improve their surface qualities. In combination with spun-glass fabric it also reinforces brittle natural stone slabs. Pre-warming the stone to 60–70°C considerably increases penetration. Not to be used below 15°C, as it will not sufficiently harden.

Wear appropriate PPE. Follow manufacturer instructions and safety regulations.